Right-o, the extra powder is not turned into gas. You might find, however, that by going to a more vigorous primer (Fed 215 or WLRM), or a mild to heavy crimp, you CAN get that extra powder to burn.

Both have the effect of changing the burn rate of the powder.

As always, when changing components or procedures, work back up. FWIW, Dutch.