The testing that I reported on was done by first soaking the primers before seating in a case for a few days, then seating the primer and also adding the testing material into the case and soaking some for over a week or two. They all fired so I guess he was lucky enough to not break the seal on the primers while seating.

Point being, just handling with clean bare hands is OK.
__________________
http://www.geocities.com/hunter18201/

Life member NAHC, Endowment Member NRA, Member Varmint Hunters Association, F.O.P. Lodge #38

Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 04:54 PM.


Powered by vBulletin® Version
Copyright ©2000 - 2013, Jelsoft Enterprises Ltd.