I shoot quite a bit of lead in my Makarov. It works just fine. The Lee mold for the 380 is reported to be completely adequate.

You'll need to use an alloy at least as hard as wheelweights in a semi-auto. I've had no trouble whatever using Lee Liquid Alox as bullet lube. Lyman doesn't list loads for that bullet, but they do have loads for a 90 and a 120-grain. Data for the 120 ought to be safe with a 102. They give max loads of: 2.1 Bullseye, 2.1 RedDot, 3.2 W231 and 2.8 Unique, among other powders. They liked W231 best for both bullets mentioned, and I like it in the Mak as well.
__________________
Freedom of the Press
Does NOT mean the right to lie!

Visit me at my Reloading Room webpage!

Get signed copies of my Vietnam novels at "Baggy Zero Four" "Mike Five Eight"
Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 05:00 AM.


Powered by vBulletin® Version
Copyright ©2000 - 2013, Jelsoft Enterprises Ltd.